INFLUENCES OF HEAT-TREATMENT ON ELECTROCHEMICAL PERFORMANCE OF NEEDLE COKE

刘鸿鹏,乔文明,张睿,詹亮,梁晓怿,凌立成
DOI: https://doi.org/10.3969/j.issn.1001-3741.2009.02.004
2009-01-01
Abstract:Needle cokes heat-treated at different temperatures were investigated by means of X-ray diffraction spectra (XRD), scanning electron microscope (SEM) and galvanostatic discharge/charge cycle tests. It was found that the degree of graphitization and the crystallite size increased with the temperature of heat-treatment, leading to quite flat morphology. Electrochemical tests demonstrated that needle coke heat-treated at 800 ℃ exhibits an initial capacity of 463 mA· h/g. After graphitization at 2 800 ℃ , the cycle performance was further improved and a reversible capacity of 360 mA· h/g was obtained after 50 cycles.