Effect of Annealing Treatment on Microstructur and Properties of Ultrafine-grained Cu-Cr Alloy

LI Ming-shan,WANG Qing-juan,DU Zhong-ze
2007-01-01
Abstract:Cu-0.4Cr alloy was pressed by equal channel angular pressing(ECAP) for 8 passes,the isometric microstructure whose size is 500 nm was obtained,then the high performance Cu-0.4Cr alloy was annealed in electric resistance furnace.And Cu-0.4Cr alloy pressed by ECAP was annealed at 473~873 K for 1h,the microstructure and mechanical properties of the alloy were analyzed,its hardness and conductivity were studied.The results show that the dispersed Cr can effectively prevent the grain from growing.The conductivity and hardness of Cu-0.4Cr alloy is up to 80.3%IACS and 210.9HV after annealing at 723 K,respectively.It has the better synthetic properties.