Partition of Heavy Metals for the Fly Ashes from MSW Incinerator Before and after Melting Treatment

WANG Xue-tao,JIN Bao-sheng,ZHONG Zhao-ping
DOI: https://doi.org/10.3969/j.issn.0253-2409.2005.02.014
2005-01-01
Abstract:The influence of fly ash on partition characteristics of heavy metals before and after melting treatment was studied , including the melting temperature, melting time and the basicity. Experimental results indicate that the fixation rates of Ni, Cr, Cu and As reach the maximum at 1 200 ℃. With the exception of Zn, temperature changes have little impact on the volatilization rates of Pb, Cd and Hg. With the increase of melting time, the fixation rates of Ni, Cr, Cu and As in samples tend to level off after melting for 90 min. The volatilization rates of Pb, Cd, Hg are more than 95% and nearly reach complete volatilization in 30 min. High basicity is beneficial to the fixation of Ni, Cr, Cu and As. The changes in the basicity of fly ash exert little influence on volatilization of Pb, Cd, Hg and Zn. Low basicity has remarkable effect on volatilization of Zn.
What problem does this paper attempt to address?