Abstract:A novel β type Ti-35wt%Nb-2.5wt%Sn/5wt%Hydroxyapitite(HA) which is biocompatible composite without Al,V noxious elements was fabricated by pulsed current activated sintering(PCAS) at 1 100 ℃ under 60 MPa using high energy mechanical milling(HEMM).The microstructures of Ti35Nb2.5Sn/10HA powder particles and bulk composite sintered from the milled powders were studied.Results indicated that ball milling to 8 h led to the α-Ti phase transform into β-Ti phase,after ball milling for 12 h,almost all Ti transform into β-Ti phase,the particle size of composite powders ball milled for 12 h was just about 500 nm,the particle size of sintered composite was about 200 nm,so nanostructure particles were obtained.The hardness and relative density of the sintered composites both increase with increasing the ball milling time.
What problem does this paper attempt to address?