Upconversion Luminescence of Kznf3 : Er3+,Yb3+ Synthesized by Hydrothermal Method

SL Zhao,YB Hou,XJ Pei,Z Xu,XR Xu
DOI: https://doi.org/10.1016/s0925-8388(03)00678-9
IF: 6.2
2004-01-01
Journal of Alloys and Compounds
Abstract:KZnF3:Er3+,Yb3+ was prepared by hydrothermal synthesis. For all samples (ErYb0–ErYb4), Er3+ concentration was fixed at 0.5 mol.%. Yb3+ concentration was changed from 0 to 4 mol.%. We observed upconversion luminescence at 653 and 553 nm (525 nm) when the samples were excited by 980 nm light. All samples were annealed at 400°C under vacuum of 10−5 Torr for 1 h. The upconversion intensity that was measured in the same condition changed when the sample was annealed. The upconversion mechanism of annealed samples is a two-photon process.