Study of Green Environment-Friendly Urea-Formaldehyde Resin for Wood-Based Panel

张跃,叶涛,刘建武,严生虎,沈介发
DOI: https://doi.org/10.3969/j.issn.2095-0411.2009.01.001
2009-01-01
Abstract:The process of the weak alkali-weak acid-weak alkali was used this study.On the basis of the tradition technology of adding urea in one potion to synthesize urea-formaldehyde resin,urea and formaldehyde were by the method of added in batches,multi-point section,which was controlled to decrease the free formaldehyde of the ura-formaldehyde resin.Individual factor experiments were carried out,which studied the influence of the F/U molar ratio,the first adding urea temperature,the polymerization reactivity time,modifier and so on.The optimum condition was obtained: the F/U molar ratio 1.31∶1,controlling the first adding urea temperature at 95-98 ℃,polymerization reactivity pH for 4.8-5.1.The free formaldehyde of synthesized urea-formaldehyde resin was less than 0.1%.Finally,the resin could reach the national E0 level standard of resin used for wood-based panel.
What problem does this paper attempt to address?