Improvement of cracking resistance of hot-dip Zn-Al-Mg coatings by heat treatment

Minyun Xu,Zhaoyang Zheng,Dong Han,Ruina Ma,An Du,Yongzhe Fan,Xue Zhao,Xiaoming Cao
DOI: https://doi.org/10.1016/j.mtcomm.2023.106521
IF: 3.8
2023-07-08
Materials Today Communications
Abstract:Hot-dip Zn-6Al-3Mg (ZAM) coatings have superior corrosion resistance; however, their cracking resistance is not ideal. In the present study, the cracking resistance of ZAM coatings was enhanced by heat treatment, and sufficient corrosion resistance was ensured. The ZAM coatings, heat-treated at 200, 270, and 340 °C, were termed ZM2, ZM3, and ZM4, respectively; the original coating was termed ZM1. The microstructure and properties of ZM2 did not change during the heat treatment. At higher heat treatment temperatures (270 and 340 °C), the MgZn 2 phase in the original coating (ZM1) transformed into the Mg 2 Zn 11 phase. The indentation tests indicated that Mg 2 Zn 11 has a better plasticity and lower hardness than those of the MgZn 2 phase. Obvious cracks appeared in the MgZn 2 phase upon completion of the test. In the bending test, ZM3 exhibited the lowest degree of cracking. The results obtained from the salt spray test indicated that the heat treatment did not reduce the corrosion resistance of the coating.
materials science, multidisciplinary
What problem does this paper attempt to address?