Microstructure Twinning and Mechanical Properties of Laser Melted Cu-10Sn Alloy for High Strength and Plasticity
Peng Yang,Xingye Guo,Dingyong He,Wei Shao,Zhen Tan,Hanguang Fu,Zhenlu Zhou,Xiaoya Zhang
DOI: https://doi.org/10.1007/s11665-021-06409-5
IF: 2.3
2021-11-17
Journal of Materials Engineering and Performance
Abstract:A dense Cu-10Sn alloy bulk specimen was obtained by optimizing the laser powder bed fusion (L-PBF) processing, and the relative density of the specimen reached 99.7%. The grain morphology was mainly the columnar dendrite and inter-dendritic phases generated along the solidification direction. Tensile testing and detailed microstructural characterization were carried out on specimens in the as-built and heat-treated condition. Under the quasi-static tensile condition, the yield strength (σ0.2), ultimate tensile strength (UTS), and the elongation of the as-built Cu-10Sn specimen were 392 MPa, 749 MPa and 29%, respectively. After the solution treatment at 800 °C for 4 h, and aging treatment at 400 °C for 2 hours, the microstructure of the specimen transformed from the columnar grain to equiaxed grain, the dislocation density decrease, and numerous annealing twins were observed in the heat-treated state. Therefore, the quasi-static tensile yield strength (σ0.2) of the specimen was reduced to 245 MPa. However, the UTS and the elongation were increased to 840 MPa and 56%, respectively, due to the interaction between annealing twins and equiaxed grain.
materials science, multidisciplinary