Deoxidation of Molten Steel with CaO-Al_2O_3 Based Refining Slag

Li Yang
Abstract:The deoxidization of molten steel with CaO-Al 2O 3 based refining slag was studied by methodology of quadratic orthogonal regression. The experimental results showed that the deoxidization equilibration time is 20-30 min and the equilibrium oxygen content is 0.000 8 %-0.001 2 %. The equilibrium total oxygen content was obtained when the refining slag and molten steel were equilibrium. The relationship between total oxygen content and optical alkalinity, Al 2O 3 content, CaF 2 content in the refining slag was obtained. The results showed that the total oxygen content linearly decreases with the increase of optical alkalinity and increases with the increase of the Al 2O 3 content when the deoxidizer is aluminium. The total oxygen content increases firstly, and then decreases when the CaF 2 content increases. The optimum composition of the refining slag is : CaO 57.29 %, Al 2O 3 9 %, MgO 10 %, SiO 2 8.71 % and CaF 2 15 %.
Materials Science
What problem does this paper attempt to address?