(Invited) Chemical Kinetic Method for Active-Site Quantification in Fe-N-C Catalysts and Correlation with Molecular Probe and Spectroscopic Site-Counting Methods
Jason S. Bates,Jesse J. Martinez,Melissa N. Hall,Abdulhadi A. Al-Omari,Eamonn Murphy,Yachao Zeng,Fang Luo,Mathias Primbs,Davide Menga,Nicolas Bibent,Moulay Tahar Sougrati,Friedrich E. Wagner,Plamen Atanassov,Gang Wu,Peter Strasser,Tim-Patrick Fellinger,Frederic Jaouen,Thatcher W. Root,Shannon S. Stahl
DOI: https://doi.org/10.1149/ma2024-01362068mtgabs
2024-08-09
ECS Meeting Abstracts
Abstract:Heterogeneous catalysts consisting of iron cations incorporated into nitrogen-doped carbon (“Fe-N-C”) have received extensive attention as leading alternatives to Pt for the electrochemical oxygen reduction reaction (ORR). Fe-N-C catalysts host mononuclear nitrogen-ligated active centers, FeN x , that frequently coexist with agglomerated Fe species. Although FeN x are the dominant active centers for ORR and other electrocatalytic reactions, the relative accuracies of methods to quantify them are still debated. Here, we develop a kinetic probe-reaction approach to quantify FeN x centers and compare it with spectroscopic and molecular probe methods. Model Fe-N-C catalysts were synthesized to contain mononuclear FeN x species at low loadings (0.1–0.4 wt% bulk Fe) on solvent-accessible surfaces using a postsynthetic metalation approach and their Fe speciation was confirmed by low-temperature 57 Fe Mössbauer spectroscopy. The initial rate of oxidation of a water-soluble hydroquinone molecule (per g catalyst ) catalyzed by these model materials correlates linearly with their density of FeN x centers, reflecting their intrinsic turnover frequency (TOF) for this reaction. This TOF, in turn, enables the estimation of the active-site density on any other Fe-N-C catalyst through a simple rate measurement. Kinetically determined FeN x site densities are measured on a suite of fourteen Fe-N-C catalysts with diverse synthetic origins and Fe speciation (0.3–8.4 wt% bulk Fe) and are compared with those estimated by low-temperature 57 Fe Mössbauer spectroscopy, CO pulse chemisorption, and electrochemical stripping of NO derived from NO 2 − . Kinetic quantifications of FeN x centers correlate well with those obtained from the CO pulse chemisorption method and Mössbauer spectroscopy. The broad survey of Fe-N-C materials also reveals the presence of outliers and challenges associated with each site quantification method. The kinetic method developed here does not require pretreatments that may alter active-site distributions nor specialized equipment beyond reaction vessels and standard analytical instrumentation, offering an attractive complementary approach. Figure 1