Synthesis of fibrous titanium silicalite (FTS-1) zeolite

K.T. Jung,J.H. Hyun,Y.G. Shul,D.S. Kim
DOI: https://doi.org/10.1016/s0144-2449(97)00063-8
1997-08-01
Zeolites
Abstract:Fibrous titanium silicalite (FTS-1) zeolite has been prepared from titanium silicalite (TS-1) particles that were less than 120 nm in diameter. The formation of FTS-1 was mainly affected by the particle size of the TS-1 zeolite. FTS-1 is formed by both capillary force and dehydroxylation among the TS-1 particles during the drying and evaporation process of the dispersed TS-1 particles in aqueous solution. The average length and the aspect ratio (length/diameter) of FTS-1 are 2.2 and mm 50~70, respectively. The obtained FTS-1 shows a two-dimensionally aligned surface that is affected by the treatment of dispersed TS-1 particles in aqueous solution. 29Si MAS n.m.r. spectra showed that the concentration of the hydroxyl group on the surface of TS-1 particles was decreased after the formation of FTS-1 and was reduced continuously up to 750 °C with calcination. This suggests that the condensation reaction of hydroxyl groups on the surface of TS-1 particles occurs by drying and heat treatment. After calcination at 750 °C, FTS-1 still exhibited characteristics of MFI-type structure with orthorhombic symmetry. It showed distinctive secondary pores due to the aggregation of TS-1 particles. This method of FTS-1 formation may suggest a new method for the preparation of various types of zeolites.
English Else
What problem does this paper attempt to address?