Effect of laser and coating surface treatment on the bond strength of zirconia ceramics

Qiao Du,Guangliang Niu
DOI: https://doi.org/10.7518/hxkq.2024.2023369
2024-06-01
Abstract:Objectives: This study aims to investigate bond strength between zirconia and resin cement through surface treatments with Er: YAG laser, Nd: YAG laser, and Si-Zr coating. Methods: Seventy-five round pre-sintered zirconia discs with a diameter of 18 mm and a thickness of 1.5 mm were prepared by a powder compactor. Fifty discs were randomly divided into five groups of 10 discs each and were subjected to five surface treatments: no treatment (control group), sandblasting with alumina particles (sandblasting group), Er: YAG laser treatment (Er: YAG laser group), Nd:YAG laser treatment (Nd: YAG laser group), and Si-Zr coating treatment (Si-Zr coating group). The discs were then bonded to composite resin columns with resin cement. The shear bond strength of each group was tested with a universal tester. Roughness tester, scanning electron microscope (SEM), and energy dispersive spectroscopy were used to analyze surface performance. Results: The bond strength of the Si-Zr coating group was higher than that of the remaining groups (P<0.05). The difference in bond strength between the sandblasting group and the Er: YAG laser group was not statistically significant (P>0.05), but both of them had higher bond strength than the Nd: YAG laser group (P<0.05). The Si-Zr coating group had the highest surface roughness (P<0.05). The surface roughness of the sandblasting, Er: YAG laser, and Nd: YAG laser groups was higher than that of the control group (P<0.05), but the difference among the three groups was not statistically significant (P>0.05). SEM observations showed irregular scratches on the surface of the sandblasting group and large pits with holes on the surface of the Er: YAG and Nd: YAG laser groups. In the Er: YAG laser group, the crystal structure was replaced by a smooth surface with a large amount of microcracks due to partial melting. Complex porous structures that comprised "island-like" structures and mass pores among the grains were observed on the surface of the Si-Zr coating. Only Zr, O, and Y were detected on the surfaces of the control, Er: YAG laser, and Nd: YAG laser groups. Al was found on the surface of the sandblasted group, and a higher proportion of Si was detected on the surface of the Si-Zr coating group. Conclusions: Er: YAG laser and Nd: YAG laser treatment on the zirconia ceramic surface could increase roughness and improve the bond strength to resin cement. Si-Zr coating treatment is an effective alternative for increasing the roughness and bond strength of zirconia surface and is superior to sandblasting and laser treatments.
What problem does this paper attempt to address?