Abstract:Diamonds produced using chemical vapor deposition (CVD) have found many applications in various fields of science and technology. Many applications involve polycrystalline CVD diamond films of micron thicknesses. However, a variety of optical, thermal, mechanical, and radiation sensing applications require more bulky CVD diamond samples. We report the results of a magnetic resonance and structural study of a thick, sizable polycrystalline CVD diamond disc, both as-prepared and treated with e-beam irradiation/high-temperature annealing, as well as gamma irradiation. The combination of various magnetic resonance techniques reveals and enables the attribution of a plentiful collection of paramagnetic defects of doublet and triplet spin origin. Analysis of spectra, electron, and nuclear spin relaxation, as well as nuclear spin diffusion, supports the conclusion of significant macro- and micro-inhomogeneities in the distribution of nitrogen-related defects.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,metallurgy & metallurgical engineering
What problem does this paper attempt to address?
The main focus of this paper is to study the magnetic resonance properties of large-sized diamond discs prepared using the Chemical Vapor Deposition (CVD) method. CVD diamond has wide applications in various scientific and technological fields such as optics, thermics, mechanics, and radiation sensing. In this study, the authors performed magnetic resonance (including Electron Paramagnetic Resonance (EPR) and Nuclear Magnetic Resonance (NMR)) and structural analysis on both untreated and electron beam irradiated/high temperature annealed, as well as gamma irradiated diamond discs. Through these techniques, they detected and differentiated various nitrogen-related spin defects in bi- and tri-stable states, and found non-uniform distributions of nitrogen-related defects at macroscopic and microscopic levels. The paper points out that although CVD diamond is commonly used for thin-film applications, future optical, thermic, and sensor applications will require thicker diamond. The studied sample was a CVD diamond disc with a diameter of 50 millimeters and a thickness of approximately 560 micrometers, and understanding the growth conditions and defect structures is crucial for characterizing its properties. EPR and NMR measurements revealed the non-uniform distribution of nitrogen-related defects, while X-ray Diffraction (XRD) provided crystallographic structural information indicating significant (111) growth orientation of diamond grains. In conclusion, this paper aims to address how to study the defect structures, particularly nitrogen-related defects and their distributions, in CVD diamond in detail using magnetic resonance techniques, in order to optimize its performance in various applications.