Abstract:Purpose To measure the effect of daily immersion in varying beverages (distilled water, tea, carbonated beverage, and orange juice) on surface roughness and color stability of 3D‐printed denture base resins. Materials and Methods 160 acrylic resin discs (15 × 2.5 mm) were made from heat‐polymerized (HP), and 3D‐printed resins (FormLabs, ASIGA, and NextDent). Resin discs (N = 40) were immersed in different solutions (distilled water, tea, carbonated beverage, or orange juice; (n = 10/group)). Surface roughness (Ra, μm) was measured initially (T0), 6 months post immersion (T1), and 12 months post immersion (T2) using a non‐contact profilometer. Color change (∆E00) was calculated using CIEL2000 at T1 and T2 using a spectrophotometer. The data were analyzed using Mann‐Whitney U test and Kruskal‐Wallis test in addition to general linear modeling (α = 0.05). Results Significant differences in surface roughness (Ra) were found between the baseline and immersion in distilled water, carbonated beverage, and orange juice (p 0.05). Noticeable color changes were observed after immersion in tea, carbonated beverage, and orange juice. All resins exceeded perceptibility and acceptability thresholds at T1 and T2. The combined effect of time and resin on color change was statistically significant (p
dentistry, oral surgery & medicine