Abstract:The large strain cavitation stemmed from the fragmentation of the highly oriented amorphous network in the quenched ultra high molecular weight polyethylene was investigated as a function of deformation temperature. The critical stress for initiating such cavitation was found to be dependent on the deformation temperature (T d ) in a way being constant below T d of 90 °C but increased with T d above 90 °C. This peculiar deformation temperature dependency of critical stress for the large strain cavitation stress was found to be associated with the activation of the αⅡ-relaxation in the deformed samples. The αⅡ-relaxation temperature increased with the increase of T d , which was attributed to the increase of the stability of the fibrils formed at large strain. The difference between αⅡ-relaxation temperature and deformation temperature showed a one-to-one correspondence to the critical stress of large strain cavitation indicating a stress was required to activate the αⅡ-relaxation at a selected T d to initiate failure of the oriented network so that cavitation in the large strain regime.
polymer science
What problem does this paper attempt to address?