Localized Charge Accumulation Driven by Li + Incorporation for Efficient LED Phosphors with Tunable Photoluminescence

Yibo Chen,Jinquan Chen,Jinhui Liang,Jin He,Zhao-Qing Liu,Yadong Yin
DOI: https://doi.org/10.1021/acs.chemmater.0c02547
IF: 10.508
2020-09-24
Chemistry of Materials
Abstract:Mn<sup>4+</sup> ion-doped red-emitting oxides are promising candidates for light-emitting-diode phosphors, but the formation and stabilization of Mn<sup>4+</sup> in the oxide matrix remain a challenge due to the spontaneous reduction of Mn<sup>4+</sup> to Mn<sup>2+</sup>. In this work, we demonstrate that the incorporation of Li<sup>+</sup> can regulate the valence of Mn ions doped in spinel-phase ZnAl<sub>2</sub>O<sub>4</sub> and enable tuning of the luminescence of Mn<sup>2+</sup> and Mn<sup>4+</sup> dopants. Both experimental and calculation results show that the incorporation of Li<sup>+</sup> ions can lead to localized charge accumulation around themselves, thereby consuming the excess charges and suppressing the self-reduction of Mn<sup>4+</sup>. This finding allows for the realization of pure red emission of Mn<sup>4+</sup> in ZnAl<sub>2</sub>O<sub>4</sub> for the first time and the fabrication of a corresponding warm white-light-emitting-diode prototype. The Li<sup>+</sup>-dependent dual emission of Mn<sup>2+</sup> (green) and Mn<sup>4+</sup> (red) co-doped in ZnAl<sub>2</sub>O<sub>4</sub> can be conveniently utilized to design a ratiometric optical thermometer with excellent visual responses. This work not only offers new atomistic insights into regulating the valence state of Mn ions but also provides an effective method for improving the performance of Mn<sup>4+</sup>-activated light-emitting-diode phosphors and devising a good phosphorescent probe for fluorescence-intensity-ratio temperature sensing.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acs.chemmater.0c02547?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acs.chemmater.0c02547</a>.Characteristics of the strongest XRD peak for L-ZAO:Mn; concentrations of elements for ZAO:Mn and L-ZAO:Mn determined by ICP-MS; Rietveld profiles and results of 0–20 wt % L-ZAO:Mn; SEM images of 0–20 wt % L-ZAO:Mn; PL spectra of ZAO and PL spectra of 0–20 wt % L-ZAO:Mn samples; XRD patterns and PL spectra of N-ZAO:Mn and K-ZAO:Mn; PL spectra of ZnAl<sub>2</sub>O<sub>4</sub>:Mn prepared with <i>x</i> wt % MgF<sub>2</sub>; decay curves and lifetimes of 0–15 wt % L-ZAO:Mn samples (λ<sub>ex</sub> = 322 nm, λ<sub>em</sub> = 651 nm); diffuse reflection spectra of 0–15 wt % L-ZAO:Mn and ZAO matrix; XPS spectra of Zn 2p, Al 2p, and O 1s in ZAO:Mn and 15 wt % L-ZAO:Mn; XRD patterns and PL spectra of O-ZAO:Mn and LO-ZAO:Mn; XRD patterns of 15 wt % L-ZAO:Mn at 300–875 K; PL spectra and color coordinates of the 15 wt % L-ZAO:Mn sample at 298–423 K; calculated band gap of ZAO with the DRS data; integrated PL intensity of the 15 wt % L-ZAO:Mn sample in the heating and cooling cycle; XRD patterns and PL spectra (λ<sub>ex</sub> = 426 nm) of 5, 8, and 10 wt % L-ZAO:Mn; FIR values at 298 or 423 K in each cycle; and supplemental illustration of the charge balance (<a class="ext-link" href="/doi/suppl/10.1021/acs.chemmater.0c02547/suppl_file/cm0c02547_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,chemistry, physical
What problem does this paper attempt to address?