Commercial Grade of P(3HB‐co‐3HHX) Final Properties Adjustment by the Modification of Cooling Conditions in the Injection Molding and Ageing Process

Juan Ivorra‐Martinez,Jaume Gomez‐Caturla,Miguel Angel Peydro,Miguel Angel Selles,Teodomiro Boronat
DOI: https://doi.org/10.1002/mame.202400033
2024-03-09
Macromolecular Materials and Engineering
Abstract:Study poly(3‐hydroxybutyrate‐co‐3‐hydroxyhexanoate) for industrial applications by change in the manufacturing and storage conditions has significant influence in mechanical properties, shrinkage, and color attributes. These alterations stem from modifications in crystallinity as observed in the tested samples. This was possible with the crystalline phase increase with a higher mold temperature and also with high temperature storage. Poly(3‐hydroxybutyrate‐co‐3‐hydroxyhexanoate) is a polymer obtained by bacterial fermentation that emerges as an alternative to polymers of petrochemical origin. The complex crystallization kinetics that occurs over 15 days after melting, known as ageing, limits its industrial application. During the aging process, there is a change of the degree of crystallinity, which has an effect on the chemical structure of the material. Additionally, changes in the mechanical properties, colorimetry, and dimensional shrinkage are observed. Different material properties are observed depending on the cooling conditions employed. For the ageing process, two different conditions are considered: ageing at room temperature and annealing at high temperature (60 °C).
materials science, multidisciplinary,polymer science
What problem does this paper attempt to address?