Quantification of lithium dendrite and solid electrolyte interphase (SEI) in lithium-ion batteries

Hanying Xu,Ce Han,Wenting Li,Huiyu Li,Xinping Qiu
DOI: https://doi.org/10.1016/j.jpowsour.2022.231219
IF: 9.2
2022-05-01
Journal of Power Sources
Abstract:The unexpected plating of lithium on the anode is a common issue for lithium-ion batteries (LIBs), which shortens the cycle life by consuming active Li+ and causes the severe safety hazard due to the formation of Li dendrites. However, the quantitive detection of deposited metallic Li is hindered by the lack of feasible and precise method. Herein, we utilized the differential scanning calorimetry (DSC) technique to quantify the deposited metallic Li by measuring the heat of metallic Li melting. This technique provides an accurate quantification method for the "dead Li" and solid electrolyte interphase (SEI) evolution of the graphite electrode. The measured minimum amount of metallic Li reaches 0.19 μg (0.72 μAh). We found that SEI growth consumes more capacity in the period of the nucleation of lithium dendrites than that in the period of the growth of lithium dendrites. The formation of SEI is the main cause for the capacity loss during the Li plating/stripping on both graphite and copper electrodes. Only 1.4–1.6% of capacity loss of the commercial pouch cell aged at low temperature is consumed to form "dead Li".
energy & fuels,materials science, multidisciplinary,electrochemistry,chemistry, physical
What problem does this paper attempt to address?
### What problems does this paper attempt to solve? This paper aims to solve the problem of quantitative detection of lithium metal deposition and solid - electrolyte interface (SEI) in lithium - ion batteries (LIBs). Specifically, the research focuses on: 1. **Formation of Lithium Dendrites**: The unexpected deposition of lithium dendrites on the negative electrode will shorten the cycle life of the battery and bring serious safety hazards due to the formation of lithium dendrites. Lithium dendrites not only consume active Li⁺, but may also penetrate the separator, leading to an internal short - circuit and then triggering thermal runaway. 2. **Excessive Growth of SEI**: The excessive growth of SEI will also consume a large amount of active Li⁺ and electrolyte, resulting in battery capacity decay. The formation and growth mechanism of SEI is complex and random. Especially under low - temperature conditions, the growth of SEI has a particularly significant impact on the capacity loss of graphite electrodes. 3. **Quantification of "Dead Lithium"**: The part of lithium dendrites that breaks off and is wrapped by SEI and loses electrical contact is called "Dead Lithium". This lithium cannot participate in further electrochemical reactions, resulting in irreversible capacity loss. Accurately quantifying the amount of "Dead Lithium" is crucial for studying the failure mechanism and safety of lithium - ion batteries. To solve these problems, the author introduced differential scanning calorimetry (DSC) to quantify the deposited metallic lithium and its heat of fusion, thus providing an accurate quantification method for measuring the evolution of "Dead Lithium" and SEI. Through this method, the author was able to detect as little as 0.19 μg (0.72 μAh) of metallic lithium deposition and found that the formation of SEI is the main cause of capacity loss during lithium deposition, especially during lithium nucleation, where SEI consumes more capacity. In addition, the author also studied the proportion of "Dead Lithium" in commercial pouch batteries during low - temperature aging. The results showed that it accounted for only 1.4 - 1.6% of the total capacity loss, indicating that the formation of SEI plays a dominant role in capacity decay. ### Key Formulas - Relationship between the heat of fusion and mass of pure metallic lithium: \[ Q(\text{mJ}) = 396.1\times m(\text{mg}) \] where \(Q\) is the heat of fusion (in mJ) and \(m\) is the mass of metallic lithium (in mg). Through these studies, the author provides important theoretical basis and technical support for the safety and life improvement of lithium - ion batteries.