Intrinsic-designed Polyimide Dielectric Materials with Large Energy Storage Density and Discharge Efficiency at Harsh Ultra-high Temperatures

Ya-Ya Tian,Ming-Sheng Zheng,Yuchao LI,Chuqi Xu,Yiyi Zhang,Wei Liu,Zhi-Min Dang,Jun-Wei Zha
DOI: https://doi.org/10.1039/d3mh01267k
IF: 13.3
2023-09-22
Materials Horizons
Abstract:Polymer dielectric materials with excellent temperature stability are urgently needed for the ever-increasing energy storage requirements in harsh high-temperature conditions. In this work, a novel diamine monomer (bis(2-cyano-4-aminophenyl)amine) was successfully synthesized to prepare a series of cyano-containing polyimides (CPI-1~3), which resulted in excellent dielectric properties and high thermostability. The maximum dielectric permittivity was up to 5.5 at 102 Hz for CPI-3, being 2.5 times higher than that of commercially used BOPP. In comparison, the CPI-1 exhibited an outstanding breakdown strength of 433 MV m -1 and a high energy density of 2.5 J cm -3 even at 250 o C, which was the highest value reported under the same condition. The synthesized CPIs through such an intrinsic approach provided a potential candidate material for energy storage and even other applications under simultaneously harsh electrical and thermal conditions.
materials science, multidisciplinary,chemistry
What problem does this paper attempt to address?