Significantly Improved High-Temperature Charge-Discharge Efficiency of All-Organic Polyimide Composites by Suppressing Space Charges

Qi-Kun Feng,Di-Fan Liu,Yong-Xin Zhang,Jia-Yao Pei,Shao-Long Zhong,Hui-Yi Hu,Xin-Jie Wang,Zhi-Min Dang
DOI: https://doi.org/10.1016/j.nanoen.2022.107410
IF: 17.6
2022-01-01
Nano Energy
Abstract:In order to satisfy the miniaturization trends of power electronic devices and safe operation in harsh environments, high-temperature dielectric polymers with excellent energy density and great reliability are desired in advanced electronic and power systems as electrostatic capacitors. Herein, the all-polymer dielectric composite films, consisting of ferroelectric polymer poly(vinylidene fluoride-co-hexafluoropropylene) (P(VDF-HFP)) as filler and linear polymer polyimide (PI) as matrix, were fabricated by in situ polymerization method for electrostatic energy storage scenarios. Scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS), and X-ray diffraction (XRD) results indicated that the P(VDF-HFP) was successfully compounded into the PI matrix. The dielectric permittivity of PI/P(VDF-HFP) energy storage composites was enhanced, while the breakdown strength and electrical resistivity values were wrecked slightly with enhancive mass fraction of P (VDF-HFP). Consequently, the discharged energy density (U-d) of PI-10, PI-20 and PI-30 were 2.60, 2.90, and 3.16 J/cm(3) at 30 C and 400 MV/m, respectively, which were 1.05, 1.17 and 1.27 times than those of neat PI film (2.48 J/cm(3)). Notably, an interesting phenomenon was observed that the charge-discharge efficiency (eta) of all organic composites was dramatically improved situated in high-temperature conditions. When the mass ratio of P (VDF-HFP) to PI was 1:4, the corresponding Ud and eta of PI-20 could be significantly improved to 2.25 J/cm(3) and 76.9% at 382 MV/m and 150 C, which were 6.7 and 10.5 times than those of neat PI film (0.336 J/cm(3) and 7.3%) at 300 MV/m, respectively. Impressively, PI-30 film delivers an enhanced Ud of 1.81 J/cm(3) and eta of 71% at 200 C and 308 MV/m. The significant improvement in the efficiency of composites under high-temperature environment is attributed to the suppression of space charges, which was verified by the TSDC results. In addition, the all-polymer composites exhibited outstanding cycling stability under harsh conditions of high temperature and high electric field. Our fabricated PI/P(VDF-HFP) composite films present potential energy storage applications in the high temperature environments with demand for flexible dielectric materials with upgraded permittivity, excellent energy density as well as reliable cycling stability.
What problem does this paper attempt to address?