Microstructure and superior mechanical property of in situ (TiBw + TiCp)/Ti composites with laminated structure

Hao Wu,Chengxin Lei,Yan Du,Wangtu Huo,Yusheng Zhang,Lian Zhou
DOI: https://doi.org/10.1016/j.ceramint.2020.12.269
IF: 5.532
2021-04-01
Ceramics International
Abstract:<p>The strength and ductility of titanium matrix composites (TMCs) hardly co-exist and show a trade-off between each other. In order to balance the strength and ductility of TMCs, <em>in situ</em> TiB whiskers (TiBw) and TiC particles (TiCp) strengthened Ti composites with laminated structure were constructed via electrophoretic depositing (EPD) boron (B) powders + graphene oxides (GOs) on pure Ti foils followed by spark plasma sintering (SPS). The experiment results reveal that increasing EPD duration leads to more synthesized TiBw + TiCp reinforcements accompanied by decreased grain size of Ti matrix in the sintered composites, which favorably results in gradually enhanced strength. A maximum yield strength (YS) of 569 MPa is achieved in the laminated composite, which is 75.6% higher than that of pure Ti sample (YS: 324 MPa). Meanwhile, the composite still owns a relatively higher elongation of 12.0%. The achievement of good ductility should benefit from the laminated architecture which exerts constraint effect on crack propagation. This work provides a short cut to achieve strength-ductility synergy in TMCs.</p>
materials science, ceramics
What problem does this paper attempt to address?