Rock joint sealing experiments using an ultra fine cement grout

Rajinder Bhasin,Per Magnus Johansen,Nick Barton,Axel Makurat
DOI: https://doi.org/10.1201/9781003211341-38
2021-05-20
Abstract:Rock joint sealing experiments have been conducted in a laboratory using a bi-axial coupled shear-flow test apparatus (CSFT). The laboratory test programme was designed to investigate the penetrative potential of a grout using different water/cement ratios on joints having different joint roughness (JRC) and joint conducting aperture in different stress conditions (total normal stress, joint water pressure and grouting pressure). The results indicate that joints with a conducting aperture (e) as small as approximately 25 microns can be grouted using a stable mixture of superfine cement, water and a super plasticizer (dispersing agent). The penetration capacity of a specific cement grout depends, in addition to the joint’s characteristics, on the maximum grain size, the water/cement ratio and the injection pressure used. The tests reveal that the minimum physical aperture (E) that can be grouted corresponds to approximately four times the cement’s maximum grain size.
What problem does this paper attempt to address?