Abstract:Solution-phase hydrogen reduction reaction (SpHR) was introduced to overcome the problems of ammonia nitrogen pollution, high energy consumption, and long production flow of traditional reduction roasting. From φ-pH diagram, the increase of reaction temperature, vanadium concentration and H 2 partial pressure is beneficial to the preparation of V 2 O 3 . High purity V 2 O 3 could not be prepared by single addition catalysis and synchronous catalysis in SpHR process, and the Ni + NiSO 4 stepwise catalysis can effectively eliminate the problem of nickel wrapped in vanadium precipitates during the precipitation process. Under the optimal conditions of Ni + NiSO 4 stepwise catalysis of nickel powder dosage 5 g/L, NiSO 4 dosage 8 g/L, nickel powder catalytic time 90 min, NiSO 4 catalytic time 30 min, the precipitate with nickel content 11.15 % was obtained, and Ni catalyst can be separated by magnetic separation with nickel recovery ratio of 99.52 %. Ni 2+ in SpHR precipitates to Ni(OH) 2 and then disintegrates and reduces to Ni, and Ni + NiSO 4 stepwise catalysis includes two steps of pre-catalysis and secondary catalysis. After fourth cyclic experiment, the vanadium content of V 2 O 3 product obtained was 67.46 % (i.e. 99.21 % V 2 O 3 purity met the requirements of GB 40301–2021), the total recovery was 98.68 %, and the vanadium loss ratio was stable at 1.22 %. The process of SpHR has no ammonia nitrogen wastewater or waste gas discharge, and the price of V 2 O 3 with purity more than 99 % on the market is about 260,000 ¥/t. The stepwise catalysis SpHR has remarkable environmental benefits and economic benefits.
engineering, chemical
What problem does this paper attempt to address?