Abstract:<p>In this study, SrZrO<sub>3</sub> doped K<sub>0.5</sub>Na<sub>0.5</sub>NbO<sub>3</sub> ceramics with Cu, Sn and Mn as sintering aid are prepared to modulate the temperature stability by conventional solid-state sintering, and samples are denoted as KNNC-100xSZ, KNNS-100xSZ and KNNM-100xSZ, respectively, where x is the doping amount. The average grain size of the KNNC-12.75SZ sample was ~150nm. The dielectric constant of KNNC-13.00SZ was 2072 and its dielectric loss was 1.8% at room temperature, with a wide temperature stability range from -55 °C to 220 °C satisfying the X9R criteria. The discharge energy density of KNNC-12.75SZ reached 1.47J/cm<sup>3</sup> at room temperature; therefore, the modified KNN is a promising candidate for X9R dielectrics with a fine grain structure and potential anti-reduction capability due to the absence of variable valence elements. The modified KNN can also be applied to energy storage capacitors subjected to high working temperatures.</p>
materials science, ceramics
What problem does this paper attempt to address?