Abstract:This study investigates the dispersion and compatibility of low-entangled "dis-entangled" UHMWPE (dis-UH) in a high-density polyethylene (HDPE) matrix using solvent-free melt-blending conditions and compares it with entangled UHMWPE (eUH) in the same matrix. The findings reveal that dis-UH/HDPE exhibits a significantly lower viscosity ratio than eUH/HDPE (1 and 4, respectively), indicating a lower critical capillary number ( C a critical ), thus enhanced dispersion and compatibility. Blends with varying dis-UH content up to 20 wt.% showed homogeneity, evidenced by DSC and SEM analysis, and demonstrated improved mechanical properties by 37% in the maximum stress ( σ max ) and 38% in Young's modulus ( E ). Linear viscoelasticity assessments revealed that higher dis-UH content slowed the dynamics and increased the apparent weight average molecular weight ( M w ), consistent with previous reports for linear entangled PE. The zero-shear viscosity ( scaling with M w ( η 0 M n ) was adjusted for high polydispersity, yielding a transitional point in the scaling exponent ( n ) from 3.6 to 3 at a reptation number of entanglement segments ( M r / M e ) of ∼287, in line with theoretical predictions. To rationalize the success of the homogenization process, we propose a qualitative molecular picture inspired from the constraint release Rouse mechanism involved in the disorientation process of bi-disperse linear polymers. In the case of dis-UH/HDPE blends, with initially lower density of long-long entanglements within dis-UH, and the highest density of short-short entanglements within HDPE matrix, the formation of long-short entanglements between dis-UH and HDPE is facilitated, which results in successful homogenization process. In the contrary, the establishment of long-short entanglements in eUH/HDPE blends will require unwinding of the long-long entanglements, which holds a higher kinetic barrier compared to dis-UH/HDPE blends, leading to unsuccessful homogenization.
polymer science
What problem does this paper attempt to address?