Comparative study on potassium poisoning of Cu-CHA catalysts for NH3-SCR: Stability and transformation of Cu2+ ions

Liping Liu,Yang Gao,Songqi Cheng,Xiaodong Wu,Yue Ma,Xu Zhang,Rui Ran,Jianbo Liu,Zhichun Si,Zhibo Ren,Duan Weng
DOI: https://doi.org/10.1016/j.jece.2022.108305
IF: 7.7
2022-10-01
Journal of Environmental Chemical Engineering
Abstract:Cu-chabazite based catalysts (Cu-SSZ-13 and Cu-SAPO-34) may suffer from chemical deactivation due to the deposition of alkali impurities on the surface of wall-flow particulate filters. In this work, the resistance of two Cu-CHA catalysts to potassium poisoning was compared, and the key factors affecting preservation and evolution of Cu2+ ions were ascertained based on the experimental characterizations and DFT calculations. The feasibility of atom (Cu and H) at various sites (6MR and 8MR) in different types of zeolites (SSZ-13 and SAPO-34) upon K+ attacking was compared. The stability of isolated Cu2+ ions in the zeolite framework and the aggregates of detached copper species determined the catalytic performance of the poisoned catalysts.
engineering, chemical, environmental
What problem does this paper attempt to address?