Zone-wise low cycle fatigue behavior of AA6061-T6 similar friction stir welding

Harish Suthar,Mohit Sharma,Anirban Bhattacharya,Surajit Kumar Paul
DOI: https://doi.org/10.1016/j.ijfatigue.2024.108155
IF: 5.489
2024-01-13
International Journal of Fatigue
Abstract:Friction stir welding (FSW) introduces variations in temperature and strain distribution, resulting in diverse microstructures in and around the weld-nugget zone. This impacts the original strengthening mechanisms of the base material, especially in precipitate-hardening aluminum alloys. This study focuses on the low-cycle fatigue (LCF) behavior of base material (BM) AA6061-T6 and its FSW joint, revealing lower fatigue life in various zones of FSW joints compared to the BM. The loss of precipitate hardening in the FSW joint leads to increased fatigue damage due to process-induced softening. Specimens from the heat-affected zone (HAZ) on the advancing and retreating sides exhibit lower fatigue life than the nugget/stir zone (SZ) due to crack-susceptible boundaries. All zone-wise specimens of AA6061 FSW joints display notable cyclic strain hardening compared to the base material. SZ specimens show slightly higher stress amplitude and plastic strain energy density than HAZ specimens, attributed to larger grains in the HAZ.
materials science, multidisciplinary,engineering, mechanical
What problem does this paper attempt to address?