Phase-Dependent Reactivity of Nickel Molybdates for Electrocatalytic Urea Oxidation
Kailong Hu,Samuel Jeong,Ganesan Elumalai,Suresh Kukunuri,Jun-ichi Fujita,Yoshikazu Ito
DOI: https://doi.org/10.1021/acsaem.0c00968
IF: 6.4
2020-07-28
ACS Applied Energy Materials
Abstract:Identifying the influence of the phase of a catalyst on its reactivity is crucial for guiding the rational design of highly active electrocatalysts. Herein, we unveil the phase-dependent reactivity of nickel molybdates (NiMoO<sub>4</sub>) for the electrocatalytic urea oxidation reaction (UOR). Various NiMoO<sub>4</sub> phases, namely, α-NiMoO<sub>4</sub>, β-NiMoO<sub>4</sub>, and the hydrate NiMoO<sub>4</sub>·<i>x</i>H<sub>2</sub>O, were synthesized, and their structural characteristics and electrochemical properties were related to their electrocatalytic performance for the UOR. The NiMoO<sub>4</sub> phase was found to determine its reactivity, and phase-dependent UOR activities were observed. In particular, β-NiMoO<sub>4</sub> exhibited a higher activity and faster kinetics than NiMoO<sub>4</sub>·<i>x</i>H<sub>2</sub>O and α-NiMoO<sub>4</sub>, which was attributed to the large electrochemical surface area, low Tafel slope, and small charge–transfer resistance of β-NiMoO<sub>4</sub>. Moreover, hydrogen generation via β-NiMoO<sub>4</sub>-catalyzed urea electrolysis achieved a much lower cell voltage (1.498 V to reach 10 mA cm<sup>–2</sup>) than that required for water electrolysis (1.633 V to reach 10 mA cm<sup>–2</sup>). This work provides insights into design strategies for high-activity electrocatalysts for energy-efficient hydrogen production.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsaem.0c00968?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsaem.0c00968</a>.Calculations of thermodynamic standard cell potentials and urea consumed during CA measurements, HRTEM images, nitrogen absorption–desorption isotherms, BJH pore size distributions, DF-STEM image, UOR performance, cyclic voltammetry curves, SEM, TEM, and XPS data after durability testing, OER polarization curves and corresponding Tafel plots, and HER polarization curves (<a class="ext-link" href="/doi/suppl/10.1021/acsaem.0c00968/suppl_file/ae0c00968_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,chemistry, physical,energy & fuels