Surfactant‐Free, Size‐Controllable, and Scalable Green Synthesis of ZIF‐8 Particles with Narrow Size Distribution by Tuning Key Reaction Parameters in Water Solvent
Donggyun Kim,Jinhyeon Park,Jisoo Park,Jieun Jang,Minsu Han,Si‐Hyung Lim,Du Yeol Ryu,Jungmok You,Wenkai Zhu,Yusuke Yamauchi,Jeonghun Kim
DOI: https://doi.org/10.1002/smtd.202400236
IF: 12.4
2024-05-04
Small Methods
Abstract:Surfactant‐free and size‐controllable green synthesis of zeolitic imidazolate frameworks‐8 (ZIF‐8) particles with a narrow size distribution has been studied by controlling the reaction key parameters of temperature, concentration, pouring time, and reactant ratio, which are related to growth rate and degree of nucleation. To demonstrate the efficient utilization of nanopores according to the particle size and size distribution, an adsorption test is conducted on the ZIF‐8 nanoparticles. The proposed synthesis method is successfully applied on a large scale (2 L), showing its clear potential for various emerging applications. The chemical/physical properties and reliable performance of nanoporous materials are strongly influenced by the particle size and corresponding distribution. Among many types of MOFs, ZIF‐8, is still widely used and many studies have been conducted to control the particle size and uniformity of ZIF‐8 using surfactants and organic solvents. However, the use of surfactants and organic solvents process is expensive and may cause environmental pollution. For the first time, in this paper, a surfactant‐free, size‐controllable, and scalable green synthesis method of ZIF‐8 particles is reported using four reaction parameters (temperature, concentration, pouring time, and reactant ratio) that affect the formation of nuclei and growth of ZIF‐8 crystals. The as‐synthesized ZIF‐8 nanoparticles show great uniformity and controllable particle sizes in the wide range of 147–915 nm. In addition, a 2 L large‐scale synthesis of ZIF‐8 with narrow size distribution is developed by finely tuned particle size in water without any additives. To demonstrate the efficient utilization of nanopores according to the particle size and size distribution, an adsorption test is conducted on the ZIF‐8 nanoparticles. This study will support the synthesis of size‐controlled ZIF‐8 with narrow size distribution and their composites for achieving high performance in the emerging applications.
materials science, multidisciplinary,chemistry, physical,nanoscience & nanotechnology