Investigation of Laves Phase Dissolution and Homogenization Kinetics in IN718 with 0.4 Wt.% Si Through a Combination of Characterization and Calculations

Dattatreya Pati,Sushil Mishra,Amit K. Singh,Nishant Kumar,Manas Paliwal
DOI: https://doi.org/10.1007/s11837-024-06496-4
2024-04-10
JOM
Abstract:The investigation of IN718 alloy for aerospace and oil and gas industries aims to develop cost-effective components. One approach is using higher Si content scrap, but microstructure control is vital to prevent issues such as micro-segregation and Laves phase formation. To achieve this, a homogenization treatment is applied. In this study, as-cast IN718 alloy with 0.4 wt.% Si was subjected to experimental investigations at 1100°C, 1150°C, and 1175°C for 12 h, 36 h, 60 h, and 96 h. A unique characterization method involved scanning 2000 points and using an area-based method to derive concentration profiles for each element. The degree of homogenization was assessed by examining delta values, representing the difference between maximum and minimum solute concentrations as a function of temperature and time. The treatment at 1175°C for 96 h exhibited the lowest delta values, signifying the suitable homogenization treatment. Furthermore, a diffusion-based model was developed, which predicted the degree of homogenization and Laves phase dissolution and suggested a two-stage heat treatment (1150°C/50 h + 1230°C/35 h) for cost-effective manufacturing processes.
materials science, multidisciplinary,metallurgy & metallurgical engineering,mining & mineral processing,mineralogy
What problem does this paper attempt to address?