Depression mechanism of ZnSO4 and Na2CO3 on talc flotation

Jia-lei LI,Yin-yu MA,Guang-li LI,Zhi-cheng LIU,NING Shuai,PEI Bin,Zhao-you LANG,Rui-zeng LIU,Dian-wen LIU,Shuai NING,Bin PEI
DOI: https://doi.org/10.1016/s1003-6326(23)66203-x
IF: 3.752
2023-05-01
Transactions of Nonferrous Metals Society of China
Abstract:The depression mechanism of a combination of ZnSO4 and Na2CO3 on talc during chalcopyrite and molybdenite flotation was investigated in-depth using flotation tests, solution speciation calculations, and various characterization techniques. Flotation tests indicate that the effective depression of talc flotation occurred in the pH range of 7−9. In this pH range, speciation calculations for the mixed solution of ZnSO4 and Na2CO3 showed that the Zn5(OH)6(CO3)2 precipitate was the predominant zinc-bearing species, which was further proven by X-ray diffraction and infrared spectroscopy measurements. Zeta potential measurement highlighted that the Zn5(OH)6(CO3)2 precipitate was positively charged while the talc surface was negatively charged in the pH range where talc depression occurred. X-ray photoelectron spectroscopy and field emission scanning electron microscopy confirmed the presence of the zinc-bearing precipitate on the surface of the talc particles treated by the combination of ZnSO4 and Na2CO3. These findings suggested that heterocoagulation between the formed Zn5(OH)6(CO3)2 and talc occurred mainly due to the electrostatic attraction, thereby leading to the depression of talc flotation.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?
This paper mainly discusses the inhibition mechanism of a mixture of zinc sulfate (ZnSO4) and sodium carbonate (Na2CO3) on talc flotation in the flotation process of sphalerite and molybdenite. The study found that talc flotation was effectively inhibited when the pH value was in the range of 7-9. Within this pH range, the main zinc compound in the ZnSO4 and Na2CO3 mixed solution was precipitated as Zn5(OH)6(CO3)2. Analysis techniques such as X-ray diffraction (XRD), infrared spectroscopy (IR), and zeta potential measurement confirmed that the Zn5(OH)6(CO3)2 precipitate was positively charged, while the talc surface was negatively charged. X-ray photoelectron spectroscopy (XPS) and field emission scanning electron microscopy (FESEM) further demonstrated the existence of zinc compound precipitates on talc particles. The research suggests that the formed Zn5(OH)6(CO3)2 due to electrostatic attraction undergoes heterocoagulation with talc, thereby inhibiting the flotation of talc. The paper also points out that although the mixture of zinc sulfate and sodium carbonate can also be used for the inhibition of sphalerite and pyrite, their inhibition mechanisms have not been fully studied. In the experiment, the effects of zinc sulfate and sodium carbonate on talc, sphalerite, and molybdenite flotation were investigated by adjusting their concentrations and pH values. The results showed that this inhibitor combination had a good inhibitory effect on talc under specific conditions while maintaining good floatability of sphalerite and molybdenite, providing a theoretical basis for talc removal in the mineral industry. However, the paper did not provide a detailed explanation for the high selectivity of this inhibitor combination, which requires further research in the future.