The effect of sulfur on the leaching of Cr3+, Cr6+, Pb2+ and Zn2+ from fly ash glass

Wenfeng Song,Zewen Zhu,Jianwei Cao,Zhi Wang,Yali Chang,Ziming Wang
DOI: https://doi.org/10.1016/j.chemosphere.2022.135387
IF: 8.8
2022-10-01
Chemosphere
Abstract:This work assessed the capture and subsequent release of potentially harmful Cr(VI), Cr(III), Pb(II) and Zn(II) ions in and from dechlorinated fly ash glass. Differential scanning calorimetry, Fourier transform infrared spectroscopy, scanning electron microscopy - energy dispersive spectroscopy and inductively coupled plasma spectrometry along with other analytical techniques were used to explore the mechanism by which sulfur affected the immobilization and long-term leaching behavior of heavy metals in fly ash glass. Working with a CaO-MgO-Al<sub>2</sub>O<sub>3</sub>-SiO<sub>2</sub>-SO<sub>3</sub> system, increasing the sulfur content was found to promote the leaching of Cr but had only a minimal effect on the loss of Pb and Zn. The concentrations of Pb and Zn in the leachate were found to remain at essentially nil over time while the Cr level increased up to 64 h and then decreased. The presence of Sulfur ions degraded the glass network and this promoted the leaching of S<sup>2-</sup>, Cr<sup>3+</sup>/Cr<sup>6+</sup>, Pb<sup>2+</sup> and Zn<sup>2+</sup>. In addition, the S<sup>2-</sup> ions reacted with Pb<sup>2+</sup> and Zn<sup>2+</sup> to form needle-shaped and flocculent sulfide precipitates, thus trapping the Pb<sup>2+</sup> and Zn<sup>2+</sup>. Si<sup>4+</sup>, Ca<sup>2+</sup>, Al<sup>3+</sup> and Fe<sup>3+</sup> were also found to migrate into the leaching solution where they combined to form a dendritic flocculent that adsorbed and encapsulated Cr. This phenomenon greatly reduced the concentration of Cr in the leachate. Thus, sulfur prevented the leaching of Cr, Pb and Zn via different mechanisms.
environmental sciences
What problem does this paper attempt to address?