Performance Evaluation of Cold Metal Transfer-Based Wire Arc Additive Manufacturing of SS316L: An Effect of Weld Thermal Cycles and Heat Inputs

Saboor Fayaz Lone,Dinesh W. Rathod,Sheikh Nazir Ahmad
DOI: https://doi.org/10.1007/s11665-024-10231-0
IF: 2.3
2024-10-06
Journal of Materials Engineering and Performance
Abstract:The research investigates the metallurgical and mechanical properties of multi-layered built-up of SS316L produced through cold metal transfer-based wire arc additive manufacturing. The present study focused on varying heat input and its effect on the structural properties of built-ups. The WAAMed deposits showcase the fusion lines resembling an arc-like shape without porosity or inter-layer interfaces, and that signifies the sound and defect-free built-up fabrication. The WAAMed walls have shown a dual-phase microstructure comprising γ-austenite and δ-ferrite along with associated solidification modes. The distribution of these phases is affected by heat input variations, leading to a decline in γ-austenite concentration and a rise in δ-ferrite and micro-inclusions with higher heat inputs. Concurrently, grain size and secondary dendrite arm spacing (SDAS) escalate proportionally with increased heat input, with grain size ranging from 8.23 to 11.16 μm and SDAS from 5.68 to 8.27 μm across different heat inputs. Oxygen-based micro-inclusions also increased with an increase in heat input. Vickers microhardness assessments illustrate a decline in hardness as heat input rises. The low heat input wall exhibits an average hardness of 191.056 HV, while the high heat wall exhibits an average hardness of 171.90 HV. A 10.56% drop in hardness for a 52.88% increase in heat input is observed. Impact energy also decreased as heat input increased. For low, medium, and high heat inputs, the average impact energy from bottom to top portions of walls was 115, 97.22, and 84 J, respectively. 1.528-fold increase in heat input leading to a 1.369-fold decrease in impact energy. Reducing heat input led to significant improvements in yield strength (408.66 ± 2.21 to 361 ± 1.67 MPa) and ultimate tensile strength (630.33 ± 3.75 to 577.33 ± 1.43 MPa), corresponding to increases of approximately 12.20% and 7.56%, respectively. Conversely, percent elongation decreased from 54.26 ± 1.2 to 42.83 ± 3.9%, marking a reduction of 22.22%. Fractured specimens exhibit uniformly dispersed dimples and micro-voids, signifying ductile fracture behavior indicative of good toughness. The obtained results indicate that the lower heat input would be preferential for WAAMed built-up in the context of mechanical and microstructural properties compared to high heat input for the built-up fabrication.
materials science, multidisciplinary
What problem does this paper attempt to address?