Selective leaching of indium from spent LCD screens by siderophore desferrioxamine E

Kun Zheng,Marc F Benedetti,Rohan Jain,Bradley M Guy,Katrin Pollmann,Eric D van Hullebusch,Marc F. Benedetti,Bradley M. Guy,Eric D. van Hullebusch
DOI: https://doi.org/10.1016/j.jhazmat.2024.134013
IF: 13.6
2024-03-26
Journal of Hazardous Materials
Abstract:Given the criticality of indium (In) in high-tech applications, spent LCD screens can represent a viable secondary In resource. In this work, an innovative and alternative technology to selectively leach In from spent LCD screens using a microbial chelating agent, desferrioxamine E (DFOE), was developed. Indium was concentrated from spent LCD screens by implementing an adapted pre-treatment procedure, allowing the isolation of an indium-rich glassy fraction. During leaching, the competition between aluminum (Al) and In for complexation with DFOE leads to the precipitation of In(OH) 3 at low DFOE concentrations (12–240 μM). After adjusting the optimal conditions (fraction size: 0–36 μM, pH: 5.5, S/L ratio: 1 g/L, 25 °C), the In leaching yield reached 32%, ten times higher than Al over 90 days with 5 mM DFOE. Thus, achieving high In recovery is possible through i) prolonging leaching durations, ii) selective leaching, and iii) minimizing Al interference. This is the first attempt to selectively leach In using a selected siderophore from end-of-life products with high concentrations of non-targeted elements (i.e. Al, Si, and Ca). This study demonstrates the potential of generating indium-rich leachates, which can be subsequently processed through the GaLIophore technology for In refining.
environmental sciences,engineering, environmental
What problem does this paper attempt to address?