Abstract:Hydroborate solid electrolytes offer high ionic conductivity and are stable in contact with alkali metal anodes, but are challenging to integrate into batteries with high-voltage cathodes [1-3]. Here, we demonstrate stable dis-/charge cycling of solid-state lithium-ion batteries combining a Li 3 (CB 11 H 12 ) 2 (CB 9 H 10 ) hydroborate electrolyte with a 4 V-class LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode, exploiting the enhanced kinetic stability of the LiCB 11 H 12 -rich and LiCB 9 H 10 -poor electrolyte composition [4]. Cells with lithium metal and indium/lithium anodes achieve a discharge capacity at C/10 of ~145 mAh g –1 at room temperature and ~175 mAh g –1 at 60 °C. Indium/lithium cells retain 98% of their initial discharge capacity after 100 cycles at C/5 and 70% after 1000 cycles at C/2. Capacity retention of 97% after 100 cycles at C/5 and 75% after 350 cycles at C/2 is also achieved with a graphite anode without any excess lithium. The energy density per cathode composite weight of 460 Wh kg –1 is on par with the best solid-state batteries reported to date. [1] L. Duchêne, A. Remhof, H. Hagemann, D. Battaglia, Energy Storage Materials, 2020, 225, 782 [2] L. Duchêne, R.-S. Kühnel, E. Stilp, E. Cuervo Reyes, A. Remhof, H. Hagemann, C. Battaglia, Energy & Environ. Science, 2017, 10, 2609 [3] R. Asakura, D. Reber, L. Duchêne, S. Payandeh, A. Remhof, H. Hagemann, C. Battaglia, Energy & Environ. Science, 2020, 13, 5048 [4] H. Braun, Ryo Asakura, A. Remhof, C. Battaglia, ACS Energy Lett. in press