Theoretical Prediction and Experimental Synthesis of Zr3AC2 (A = Cd, Sb) Phases

Jia Luo,Fengjuan Zhang,Bo Wen,Qiqiang Zhang,Longsheng Chu,Yanchun Zhou,Qingguo Feng,Chunfeng Hu
DOI: https://doi.org/10.3390/ma17071556
IF: 3.4
2024-03-29
Materials
Abstract:MAX phases have great research value and application prospects, but it is challenging to synthesize the MAX phases containing Cd and Sb for the time being. In this paper, we confirmed the existence of the 312 MAX phases of Zr3CdC2 and Zr3SbC2, both from theoretical calculations and experimental synthesis. The Zr3AC2 (A = Cd, Sb) phase was predicted by the first-principles calculations, and the two MAX phases were confirmed to meet the requests of thermal, thermodynamic, and mechanical stabilities using formation energy, phonon dispersion, and the Born–Huang criteria. Their theoretical mechanical properties were also systematically investigated. It was found that the elastic moduli of Zr3CdC2 and Zr3SbC2 were 162.8 GPa and 164.3 GPa, respectively. Then, differences in the mechanical properties of Zr3AC2 (A = Cd, In, Sn, and Sb) were explained using bond layouts and charge transfers. The low theoretical Vickers hardness of the Zr3CdC2 (5.4 GPa) and Zr3SbC2 (4.3 GPa) phases exhibited excellent machinability. Subsequently, through spark plasma sintering, composites containing Zr3CdC2 and Zr3SbC2 phases were successfully synthesized at the temperatures of 850 °C and 1300 °C, respectively. The optimal molar ratio of Zr:Cd/Sb:C was determined as 3:1.5:1.5. SEM and the EDS results analysis confirmed the typical layered microstructure of Zr3CdC2 and Zr3SbC2 grains.
materials science, multidisciplinary,chemistry, physical,physics, applied, condensed matter,metallurgy & metallurgical engineering
What problem does this paper attempt to address?
The paper attempts to address the following issues: 1. **Theoretical Prediction**: Confirm the existence of two new 312 MAX phases, Zr3CdC2 and Zr3SbC2, and their thermodynamic, dynamic, and mechanical stability through first-principles calculations. 2. **Experimental Synthesis**: Successfully synthesize the two MAX phases, Zr3CdC2 and Zr3SbC2, at different temperatures using spark plasma sintering technology, and determine their layered microstructure. Specifically, the paper demonstrates the thermodynamic and mechanical stability of these two MAX phases through theoretical calculations and experimental validation, and explores their elastic modulus and Vickers hardness. Additionally, the paper optimizes the synthesis conditions, finds the optimal molar ratio (Zr:Cd/Sb:C = 3:1.5:1.5), and successfully synthesizes composites containing Zr3CdC2 and Zr3SbC2 phases at 850°C and 1300°C.