Comparative study on structural, morphological, and optical properties of MS/Fe3O4 nanocomposites and M-doped Fe3O4 nanopowders (M = Mn, Zn)

P. Soltanpour,R. Naderali,Kh. Mabhouti
DOI: https://doi.org/10.1038/s41598-024-72026-6
IF: 4.6
2024-09-14
Scientific Reports
Abstract:In the present work, the un-doped, M-doped magnetite (Fe 3 O 4 ); (M = Mn, Zn), and MS/Fe 3 O 4 composite nanopowders with a cubic spinel-type structure and average crystallite size range from 8.30 to 12.33 nm were synthesized by co-precipitation method. The FESEM images revealed the shape of particles are spherical with a grain size in the range of 33.44–49.77 nm. Through the analysis of reflectance data using Tauc's model, the direct band gap energies of 2.98 eV, 2.93 eV, 3.01 eV, 2.85 eV, and 2.95 eV were determined for Un-doped Fe 3 O 4 , Mn-doped Fe 3 O 4 , Zn-doped Fe 3 O 4 , MnS/Fe 3 O 4 composite, and ZnS/Fe 3 O 4 composite NPs respectively. The parameters such as extinction coefficient and refractive index of the nanoparticles were computed by the Kramers–Kronig (K–K) method. Non-linear optical (NLO) parameters were computed from DRS data using the Wemple–Di-Domenico (WDD) model. The calculated third-order NLO susceptibility and also electrical susceptibility represented the maximum value for MnS/Fe 3 O 4 composite NPs compared to the other samples. Considering the advanced optical parameters of MS/Fe 3 O 4 composite samples, these particles can be suitable candidates for non-linear optical applications.
multidisciplinary sciences
What problem does this paper attempt to address?