Abstract:Toxic hydrogen fluoride (HF) gas can be generated when LiPF 6 , a salt used in lithium-ion battery electrolytes, thermally decomposes and/or reacts with trace water. Simultaneous thermal analysis and mass spectrometry (STA-MS) was conducted on five different organic solvents containing LiPF 6 to determine the temperatures at which HF is generated and the activation energies of the decomposition reaction. STA-MS allows the simultaneous direct observation of electrolyte thermal stability and hydrogen fluoride generation, something that is not possible with gas chromatography–mass spectrometry alone, thus it represents a more efficient and simple experimental approach. The five solvents tested in this study were anhydrous tetrahydrofurfuryl alcohol (THFA), 1,3-dioxolane (1,3-DL), diethyl carbonate (DEC), 1,2-dimethoxyethane (DME), and ethyl carbonate (EC). STA-MS analysis of the LiPF 6 in these solvents revealed that HF generation occurred at different temperatures for each electrolyte. In the case of 1M LiPF 6 in THFA, the addition of 1000 ppm of water reduced the thermal decomposition temperature compared to solid neat LiPF 6 . Except for EC, all of the other electrolyte systems exhibited a lower HF generation temperature and a lower reaction activation energy (Ea) when water was present. Additionally, from a risk assessment perspective, the results indicate that the HF generation starts from the SEI layer decomposition stage which occurs early in the thermal runaway mechanism of the lithium-ion battery.
Environmental Science,Chemistry
What problem does this paper attempt to address?