Abstract:The microstructure and texture were investigated for nanocrystalline Au‐13at.%Pd deformed by high‐pressure torsion. The grain size of this alloy is observed to remain below about 20 nm when subjected to severe plastic deformation. Surprisingly, the initial powder compaction texture did not change significantly during shearing. The results are explained in terms of a grain boundary sliding mechanism involving planar interfaces formed by grain boundary migration. This article is protected by copyright. All rights reserved.