Advancing Sustainable Construction Materials: Wood, Rubber, and Cenospheres Geopolymer Masonry Units Development

Firesenay Zerabruk Gigar,Amar Khennane,Jong-Leng Liow,Safat Al-Deen,Biruk Hailu Tekle,Cooper J. Fitzgerald,Anthony Basaglia,Charles L. Webster
DOI: https://doi.org/10.3390/su16083283
IF: 3.9
2024-04-15
Sustainability
Abstract:As the environmental impact of modern society continues to escalate, the construction industry actively pursues environmentally friendly materials to revolutionize its practices. Recycling, especially repurposing end-of-service materials and industrial wastes, emerges as a pivotal strategy offering a promising path towards sustainable construction. This study focuses on the innovative reuse of end-of-service wood, crumb rubber, and cenosphere with geopolymer binder to produce sustainable alternatives to masonry units. The study was conducted in two stages. In the first stage, cube samples were produced and tested to establish an optimal mix design. Results indicated that as the relative volume of waste increased, the compressive strength decreased. The compressive strength of the wood geopolymer composite decreased from 25 MPa to 4 MPa as the wood-to-binder ratio increased from 0.1 to 0.5. An increasing trend was observed for density with the increase of the rubber-to-wood ratio. The compressive strength also increased with the increase of the rubber-to-wood ratio for most of the investigated ranges. As fly ash is gradually replaced by cenospheres, a significant decrease in compressive strength was noted, about 70% and 80% for wood-to-binder (ratios of 0.2 and 0.3, respectively). In the second stage, three distinct types of masonry units were produced and tested based on the optimized mix design. The compressive strength results indicated promising performance, with wood-geopolymer masonry units exhibiting a strength of 8.39 MPa, wood-rubber-geopolymer masonry units achieving 8.32 MPa, and wood-cenosphere-geopolymer masonry units resulting in 7.33 MPa. While these values fell below the target 10 MPa, it is noteworthy that wood-geopolymer masonry units and wood-rubber-geopolymer masonry units met the minimum compressive strength requirements of some standards and demonstrated significantly better ductility compared to traditional masonry units. The results showcase significant promise in the viability and performance of these innovative masonry units.
environmental sciences,environmental studies,green & sustainable science & technology
What problem does this paper attempt to address?
The problem this paper attempts to address is the growing demand for environmentally friendly materials in the construction industry, particularly how to develop sustainable building materials by recycling waste materials and industrial by-products. Specifically, the paper explores how to combine waste wood, rubber particles, and cenospheres with geopolymers to produce sustainable masonry units. The research aims to assess the feasibility of these composite materials in terms of structural performance and sustainability, and to explore their potential applications in actual construction. The paper achieves this goal through a two-stage experiment: 1. **First Stage**: Prepare cube samples and test workability and compressive strength under different mix ratios to determine the optimal mix design. The results show that as the relative volume of waste increases, the compressive strength decreases. For example, when the ratio of wood to binder increases from 0.1 to 0.5, the compressive strength of the wood-geopolymer composite decreases from 25 MPa to 4 MPa. Additionally, as the ratio of rubber to wood increases, both density and compressive strength improve. However, when fly ash is gradually replaced by cenospheres, the compressive strength significantly decreases. 2. **Second Stage**: Based on the optimized mix design, produce three different types of masonry units and test their compressive strength. The results show that the compressive strength of wood-geopolymer masonry units is 8.39 MPa, wood-rubber-geopolymer masonry units is 8.32 MPa, and wood-cenosphere-geopolymer masonry units is 7.33 MPa. Although these values are below the target of 10 MPa, the wood-geopolymer and wood-rubber-geopolymer masonry units meet some standards' minimum compressive strength requirements and exhibit better ductility. Overall, the study demonstrates the great potential of these innovative masonry units in terms of feasibility and performance, providing new ideas for the sustainable development of the construction industry.