Optimization of allotropic and hardness of aluminum oxide coating by PEO

Babak Ghorbanian,Mohammad Tajally,Seyed Mohammad Mousavi Khoie,Hossien Tavakoli
DOI: https://doi.org/10.48550/arXiv.2005.07471
IF: 2.552
2020-05-15
Chemical Physics
Abstract:One of the most important methods of producing materials and oxide coating is plasma electrolytic oxidation (PEO). Coatings made on aluminum in PEO method have two allotropes of $\alpha$-Al$_2$O$_3$ and $\gamma$-Al$_2$O$_3$. Coatings containing $\alpha$-Al$_2$O$_3$ have more hardness and wear resistance; therefore, the main goal of the present study is to optimize aluminum oxide allotrope for increasing the ratio of $\alpha$-Al$_2$O$_3$ in coating made with PEO method. Results of the present study shows that the optimum electrolyte compound for making highest phase of $\alpha$-Al$_2$O$_3$ has 2.9 g/lit of KOH, 1.15 g/lit of Na4P2O7, and 0.34 g/lit of NaAlO2 and ratio of highest allotropic pick of $\alpha$-Al$_2$O$_3$ to highest allotropic pick of $\gamma$-Al$_2$O$_3$ (in XRD test) in the optimum condition is 0.622 and hardness is 1648 Vickers.
What problem does this paper attempt to address?