Large Electrostrictive Coefficient in a Two-Dimensional Hybrid Perovskite Ferroelectric
Han-Yue Zhang,Zhi-Xu Zhang,Xiao-Gang Chen,Xian-Jiang Song,Yi Zhang,Ren-Gen Xiong
DOI: https://doi.org/10.1021/jacs.0c12907
IF: 15
2021-01-15
Journal of the American Chemical Society
Abstract:Two-dimensional (2D) hybrid organic–inorganic perovskites (HOIPs) are attracting tremendous interest for their great scientific and technological potential in photovoltaics and optoelectronics. Although the ferroelectricity in 2D HOIPs has been greatly developed, however, to date no phosphonium-based 2D HOIP ferroelectrics have yet been found. Meanwhile, electrostriction plays an important role in the electromechanical behavior of ferroelectrics, while it has never been reported for 2D HOIP ferroelectrics. Here, we present the first phosphonium-based 2D HOIP ferroelectric (EATMP)PbBr<sub>4</sub> (EATMP = (2-aminoethyl)trimethylphosphanium) with a direct bandgap of 2.84 eV. Notably, (EATMP)PbBr<sub>4</sub> possesses a high Curie temperature of 534 K, which is the highest among all reported 2D HOIP ferroelectrics. Moreover, it exhibits a large electrostrictive coefficient of about 3.96 m<sup>4</sup> C<sup>–2</sup> as well, far exceeding those of PVDF (1.3 m<sup>4</sup> C<sup>–2</sup>) and inorganic ones (∼0.034–0.096 m<sup>4</sup> C<sup>–2</sup>). With excellent ferroelectric and piezoelectric properties and the merit of easy fabrication, (EATMP)PbBr<sub>4</sub> shows great potential in applications for future smart devices of actuators, transducers, and sensors.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/jacs.0c12907?goto=supporting-info">https://pubs.acs.org/doi/10.1021/jacs.0c12907</a>.Packing view of crystal structures, distribution of atoms in the (EATMP)PbBr<sub>4</sub>, thermogravimetric analysis, dielectric responses, in-plane (lateral) PFM amplitude and phase images, vertical PFM amplitude and phase images, measured piezoelectric coefficient, powdered X-ray diffraction, point charge calculation on saturated polarization, piezoelectric and dielectric constant matrix, crystal data and structure refinement, selected bond lengths and angles, selected hydrogen-bond parameters, electrostrictive coefficient, sample preparation, and measuremental methods (<a class="ext-link" href="/doi/suppl/10.1021/jacs.0c12907/suppl_file/ja0c12907_si_001.pdf">PDF</a>)X-ray crystallographic data for (EATMA)PbBr<sub>4</sub> at 293 K (<a class="ext-link" href="/doi/suppl/10.1021/jacs.0c12907/suppl_file/ja0c12907_si_002.cif">CIF</a>)X-ray crystallographic data for (EATMP)PbBr<sub>4</sub> at 293 K (<a class="ext-link" href="/doi/suppl/10.1021/jacs.0c12907/suppl_file/ja0c12907_si_003.cif">CIF</a>)X-ray crystallographic data for (EATMP)PbBr<sub>4</sub> at 448 K (<a class="ext-link" href="/doi/suppl/10.1021/jacs.0c12907/suppl_file/ja0c12907_si_004.cif">CIF</a>)This article has not yet been cited by other publications.
chemistry, multidisciplinary