Abstract:This study examined the effect of the Sr concentration in SrK/CaO catalysts based on oyster shells for the transesterification of canola oil. The CaO support was obtained by mixing 800 °C calcined oyster shell and limestone. Then, K and Sr were impregnated simultaneously at three different Sr/(Sr + K) molar ratios, 0.2, 0.3, and 0.4, and calcined at 800 °C. XRD, SEM, and Hammett indicators were used to characterize the catalysts. The reaction conditions were 60 °C, 1 h, met/oil = 12.5, and a catalyst loading of 7 wt%. The results showed that a Sr/(Sr + K) = 0.3 produces larger K 2 Sr(CO 3 ) 2 crystals that contribute synergistically to the catalytic activity. At Sr/(Sr + K) > 0.3, the K and Sr are segregated, decreasing the alkaline character and activity. Also, the optimization of WCO transesterification conditions was carried out by Box–Behnken response surface design with SrK/CaO-0.3 catalyst. The theoretical optimal conditions were 70 °C, 1.5 h, and a met/oil = 10, which achieved 79 % of biodiesel yield. Nonetheless, the produced WCO biodiesel did not present acceptable quality, and this reactive system increased the lixiviation of the active phases.
engineering, chemical
What problem does this paper attempt to address?