Factors Affecting the Catalytic Activity of Pd/ZrO2for the Combustion of Methane

Jason N. Carstens,Stephen C. Su,Alexis T. Bell
DOI: https://doi.org/10.1006/jcat.1998.2029
IF: 7.3
1998-05-01
Journal of Catalysis
Abstract:The catalytic combustion of CH4has been investigated over Pd/ZrO2with the aim of identifying how the state of oxidation of the Pd affects the catalytic activity, particularly at low temperatures. It is found that fully reduced Pd is inactive and that the activity increases at 533 K until a plateau in activity is achieved when 6–7 ML of PdO have formed over the surface of the Pd crystallites. The maximum activity is identical to that for fully oxidized Pd. Examination of the PdO formed under reaction conditions and during oxidation in O2at 533 K reveals some differences. Temperature-programmed reduction in CH4and Raman spectroscopy demonstrate that the oxide formed under reaction conditions is largely crystalline PdO, whereas the oxide formed in O2is a mixture of amorphous and crystalline PdO. The crystalline form of PdO is found to reduce more readily than the amorphous form. It is observed that the low-temperature CH4combustion activity of PdO can be enhanced by producing a small amount of metallic Pd on the surface of PdO. The metallic Pd is more effective than PdO for the dissociative adsorption of CH4. It is hypothesized that the products of CH4adsorption on Pd, Hsand CHx,s(x=3–1), rapidly diffuse to the Pd/PdO interface and then reduce the PdO to Pd. The effects of metallic Pd cannot be sustained, though, under steady-state conditions, because the metallic Pd is oxidized back to PdO.
chemistry, physical,engineering, chemical
What problem does this paper attempt to address?