Ultrahigh energy storage density and charge‐discharge performance in novel sodium bismuth titanate‐based ceramics

Shuaishuai Bian,Zhenxing Yue,Yunzhou Shi,Jie Zhang,Wei Feng
DOI: https://doi.org/10.1111/jace.17486
IF: 4.186
2020-10-02
Journal of the American Ceramic Society
Abstract:<p>Lead‐free ferroelectric ceramics are very suitable for electrostatic energy storage capacitors due to their outstanding characteristics of high charge‐discharge speed, high power density and environmental‐friendliness. Herein, a novel material system as (1‐<i>x</i>)Na<sub>0.5</sub>Bi<sub>0.5</sub>TiO<sub>3</sub>‐<i>x</i>CaZr<sub>0.5</sub>Ti<sub>0.5</sub>O<sub>3</sub> (NBT‐CZT, <i>x</i> = 0, 0.05, 0.10, 0.12, 0.15, 0.20) was designed and prepared for dielectric energy storage ceramics. It demonstrated that the CZT additives induced a phase transition for the NBT ceramics, from ferroelectric to relaxor ferroelectric. In particular, extremely high stored energy storage density (6.92 J/cm<sup>3</sup> and 5.37 J/cm<sup>3</sup>), high recoverable energy storage density (4.77 J/cm<sup>3</sup> and 4.37 J/cm<sup>3</sup>) and moderate efficiency (69.0% and 81.4%) were achieved in both the samples of <i>x</i> = 0.12 and <i>x</i> = 0.15, respectively. The ceramics exhibited excellent stability of energy storage performance covering a wide temperature (25‐200 °C) and frequency (0.5‐50 Hz) range, and also fatigue cycles up to 10<sup>5</sup>. Additionally, the NBT‐CZT ceramics had a fast discharge speed (<i>t</i><sub>0.9</sub> &lt; 100 ns) and high power density (24.2 MW/cm<sup>3</sup>, <i>E</i> = 100 kV/cm, <i>x</i> = 0.15), and the charge‐discharge process remained stable even the measured temperature was up to 160 °C. Therefore, the NBT‐CZT ceramics have the potential to be utilized in electrostatic energy storage applications.</p>
materials science, ceramics
What problem does this paper attempt to address?