Comparative investigation of tellurium‐doped transition metal nanoparticles (Zn, Sn, Mn): Unveiling their superior photocatalytic and antibacterial activity
Misbah Umar,Humayun Ajaz,Mohsin Javed,Ali Bahadur,Shahid Iqbal,Sajid Mahmood,Afifa Sarwar,Khalid M. Alotaibi,Matar Alshalwi
DOI: https://doi.org/10.1002/bio.4799
IF: 2.613
2024-06-12
Luminescence
Abstract:We have successfully constructed both doped and undoped metal oxide NPs of Mn, Zn, and Sn utilizing the coprecipitation method. Notably, doped ZnO NPs displayed a high capacity for eliminating up to 98% of organic contaminants from wastewater. ZnO exhibited the maximum zone inhibition for gram‐positive and gram‐negative microbes, measuring 31.5 and 37.8 mm, respectively. The superior % degradation and antibacterial activity of doped and undoped ZnO NPs can be attributed to their spherical nanoparticle shape and larger surface area. In this study, tellurium‐doped and undoped metal oxide nanoparticles (NPs) (ZnO, Mn3O4, SnO2) are compared, and a practical method for their synthesis is presented. Nanocomposites were created using the coprecipitation process, and comparisons between the three material categories under study were made using a range of characterization methods. The produced materials were subjected to structural, morphological, elemental composition, and functional group analyses using XRD, FESEM in combination with EDS, and FTIR. The optical characteristics in terms of cutoff wavelength were evaluated using UV–visible spectroscopy. Catalyzing the breakdown of methylene blue (MB) dye, the isolated nanocomposites demonstrated very consistent behavior when utilized as catalysts. Regarding both doped and undoped ZnO NPs, the maximum percentage of degradation was found to be 98% when exposed to solar Escherichia coli and Staphylococcus aureus, which stand for gram‐positive and gram‐negative bacteria, respectively, and were chosen as model strains for both groups using the disk diffusion technique in the context of in vitro antibacterial testing. Doped and undoped ZnO NPs exhibited greater antibacterial efficacy, with significant inhibition zones measuring 31.5 and 37.8 mm, compared with other metal oxide NPs.
chemistry, analytical