Abstract:Expanded polystyrene (EPS) waste is generated by industry and post-consumer products. This is non-biodegradable, but is often disposed of by incineration or landfill, resulting in environmental pollution. Fly ash (FA) is a waste product from coal-fired power plants, and silica fume is a by-product of the smelting process in the production of silicon and ferrosilicon alloys. Both materials cause environmental pollution. Instead of disposing of them, there is a better way to put them to good use, such as EPS concrete (EPSC), by using EPS as a coarse aggregate and a mixture of fly ash and silica fume as a partial cement replacement. In this study, different mixes were investigated in which 100% of the coarse aggregate was replaced by EPS beads and the cement was replaced by a mixture of FA and SF at 20%, 25%, and 30%. Several laboratory tests were performed, including a slump test, a density test, a compressive strength test, and an ultrasonic pulse velocity (UPV) test. Based on the dataobtained, the optimum EPSC mix is EPSC3 (20% FA,5% SF) with 25% cement replacement and a compressive strength of 12.8 MPa at 28 days. The total slump of EPSC ranges from 65 mm to 173 mm and the total density ranges from 1562.6 kg/m3 to 1619.4 kg/m3.
What problem does this paper attempt to address?