Formic acid electrooxidation on palladium nanostructured electrodes in concentrated solutions

María A. Montero,María R. Gennero de Chialvo,Abel C. Chialvo
DOI: https://doi.org/10.1016/j.electacta.2023.143580
IF: 6.6
2023-11-28
Electrochimica Acta
Abstract:The formic acid oxidation reaction (FAO) was evaluated on palladium nanostructured films supported on glassy carbon in 0.5 M H 2 SO 4 + x M HCOOH solutions, where 0.5 ≤ x ≤ 8.0, in the potential range 0.2 ≤ Es / V ≤ 0.6 vs. RHE at 25°C. Measurements consisted in chronoamperometric experiments, which were followed by stripping voltammetry in order to evaluate the presence of CO ad . Open circuit potential (OCP) decay was also employed to analyse the formic acid spontaneous decomposition. The results of OCP experiments showed the formation of β-PdH hydride as well as the absence of CO ad for all HCOOH concentrations, evidencing that the spontaneous decomposition of HCOOH on palladium is the dehydrogenation reaction, which produces H 2 and CO 2 . It was demonstrated that CO ad is not directly involved in the kinetic mechanism of the FAO on palladium, and it was also explained the controversy related to the detection of CO ad in previous studies. Additionally, the highest FAO electrocatalytic activity was observed at x = 2.0 M.
electrochemistry
What problem does this paper attempt to address?