Graphite recovery from waste Li-ion battery black mass for direct re-use
Alexander Chernyaev,Anna Kobets,Kerli Liivand,Fiseha Tesfaye,Pyry-Mikko Hannula,Tanja Kallio,Leena Hupa,Mari Lundström
DOI: https://doi.org/10.1016/j.mineng.2024.108587
IF: 5.479
2024-01-27
Minerals Engineering
Abstract:Graphite was recovered from two leached (H 2 SO 4 = 2 M, 60 °C, t = 3 h, Fe 3+ = 2 g/L) Li-ion battery black mass concentrates with minimized energy consumption. One black mass originated from a mixture of mobile device and power tool batteries, and another from a single electric vehicle battery. The leach residues were pyrolyzed (800 °C, t = 1 h, Ar atmosphere) to remove the polyvinylidene fluoride (PVDF) binder and other non-metallic fractions. The black mass, its leach residue, and pyrolyzed residue were characterized using inductively coupled plasma-optical emission spectrometry (ICP-OES), ion chromatography (IC), scanning electron microscopy with energy dispersive X-ray spectroscopy (SEM-EDS), X-ray diffraction (XRD), thermogravimetric analysis (TGA), Raman spectroscopy, and N 2 adsorption/desorption. After hydrometallurgical recycling and pyrolysis, the main post-metallurgical black mass impurities were cobalt oxide, iron, acid-resistant boehmite (AlO(OH)), and silicon dioxide. The pyrolysis resulted in electrolyte and binder removal, affected the crystallinity of the remaining boehmite. The recovered graphite-rich residue with impurities identified was tested as an anode in half-cells vs. metal Li. The average specific capacities of recovered graphite-rich residues from both sources were 350 and 250 mAh/g at 0.1C and their capacity retention after 100 cycles was high (80 %) suggesting rather slow deterioration and hence the proposed recycling route being promising for the graphite reuse in new Li-ion batteries.
engineering, chemical,mining & mineral processing,mineralogy