Durable Machine-Washable Wool via AOX-Free Plasma-Mediated Coating with Keratin
Marwa Abou-Taleb,Hosam El-Sayed
DOI: https://doi.org/10.1080/15440478.2024.2408626
2024-10-25
Journal of Natural Fibers
Abstract:Although their favorable performance, appearance, and comfort attributes, woolen garments have the tendency to felt unenviably during washing. In this work, an eco-friendly, energy-saving, non-deteriorative process for the fabrication of machine-washable wool tops (WTs) was proposed. WTs were exposed to atmospheric air or an argon plasma treatment at different powers for various durations, followed by coating with a protein biopolymer, namely keratin, using the pad-dry-cure technique. The felting resistance of the finished WTs was evaluated, and the results revealed that the finished sample has an enhanced felting resistance to the extent of machine-washable wool (no felt ball is formed), whereas the untreated sample forms a felt ball with a diameter of 2.166 cm after undergoing the felting test. The treated WTs maintained their felting resistance after 20 wash cycles. The surface composition of the plasma-treated WTs was examined using X-ray photoelectron spectroscopy. The change in the chemical structure of the treated WTs was monitored by determining the cystine content, alkali solubility, base-combining capacity, and affinity to anionic dye. The dye exhaustion of the untreated and finished samples after 60 min was 66% and 98.8%, respectively. Scanning electron microscopy was used to study the wool fibers' topography. 尽管羊毛服装具有良好的性能、外观和舒适性,但在洗涤过程中却有令人难以忍受的感觉. 在这项工作中,提出了一种环保,节能,不变质的可机洗羊毛上衣(WT)制造工艺. 将 WT 暴露于大气或不同功率的氩等离子体处理中不同时间,然后使用垫干固化技术涂覆蛋白质生物聚合物,即角蛋白. 对成品 WT 的抗毡缩性进行了评估,结果表明,成品样品具有可机洗羊毛(不形成毡球)程度的增强抗毡缩性能,而未经处理的样品在经过毡缩测试后形成直径为2.166 cm的毡球. 经过处理的 WT 在 20 次洗涤循环后仍保持其抗毡缩性. 使用X射线光电子能谱检查等离子体处理的 WT 的表面组成. 通过测定胱氨酸含量,碱溶解度,碱结合能力和对阴离子染料的亲和力来监测处理后WTs化学结构的变化. 60分钟后,未处理和成品样品的染料耗竭率分别为 66% 和 98.8%。扫描电镜用于研究羊毛纤维的形貌.
materials science, textiles